Green Silicon Carbide Properties, Applications and Production Process
Introduction
Green silicon carbide is made of petroleum coke and high quality silica as the main raw material, adding salt as an additive, and smelted by resistance furnace at high temperature.
Production Process
Green silicon carbide is used for processing cemented carbide, glass, ceramics and non-metallic materials, as well as for semiconductor materials, high-temperature silicon-carbon rod heaters, far-infrared source substrates, etc. Green silicon carbide is manufactured in the same way as black silicon carbide, but the purity of the raw material used is higher, and it is also formed at a high temperature of about 2200°C in a resistance furnace, green, translucent and hexagonal in shape, with a higher Sic content than black.
Applications
Green silicon carbide is an inorganic salt compound with the following applications.
1, applied in the non-ferrous metal smelting industry. With green silicon carbide high temperature, strength, good thermal conductivity and impact resistance, high temperature indirect heating materials.
2, applied in the steel industry. With green silicon carbide corrosion resistance, thermal shock wear resistance and good thermal conductivity to improve the service life of large blast furnaces.
3、Application in metallurgical ore processing. Green silicon carbide has strong wear resistance, hardness second only to diamond, is the ideal material.
4、Applied to the building materials ceramic grinding wheel industry. Use its characteristics, thermal conductivity, thermal radiation and high temperature strength to make plate kiln. It can not only reduce the kiln capacity, but also improve the installed capacity of the furnace and product quality and shorten the production cycle. This is also ideal for indirect material sintering ceramic glaze baking.
5, the application of energy saving. Use its good thermal conductivity and thermal stability to make heat exchangers, saving 20% of fuel consumption and 35% of fuel and increase productivity by 20-30%.